Juntavee N, Attashu S. Effect of different sintering process on flexural strength of translucency monolithic zirconia. J Clin Exp Dent. 2018;10(8):e821-30.

 

doi:10.4317/jced.54749

http://dx.doi.org/doi:10.4317/jced.54749

 

References

1. Conrad HJ, Seong WJ, Pesun IJ. Current ceramic materials and systems with clinical recommendations: a systematic review. J Prosthet Dent. 2007;98:389–404.
https://doi.org/10.1016/S0022-3913(07)60124-3

 

2. Denry I, Kelly JR. Emerging ceramic-based materials for dentistry. J Dent Res. 2014;93:1235–42.
https://doi.org/10.1177/0022034514553627
PMid:25274751 PMCid:PMC4237640

 

3. Kohorst P, Junghanns J, Dittmer MP, Borchers L, Stiesch M. Different CAD/CAM-processing routes for zirconia restorations: influence on fitting accuracy. Clin Oral Investig. 2011;15:527–36.
https://doi.org/10.1007/s00784-010-0415-9
PMid:20495937

 

4. Guazzato M, Albakry M, Ringer SP, Swain MV. Strength, fracture toughnessand microstructure of a selection of all-ceramic materials. Part ii. Zirconia-based dentalceramics. Dent Mater. 2004;20:449-56.
https://doi.org/10.1016/j.dental.2003.05.002
PMid:15081551

 

5. Tinschert J, Natt G, Mautsch W, Augthun M, Spiekermann H. Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: A laboratory study. Int J Prosthodont. 2001;14:231-8.
PMid:11484570

 

6. Hannink RJ, Kelly PM, Muddly BC. Transformation toughening in zirconia containing ceramics. J Am Ceram Soc. 2000;83:461–87.
https://doi.org/10.1111/j.1151-2916.2000.tb01221.x

 

7. Lughi V, Sergo V. Low temperature degradation-aging-of zirconia: A critical review of the relevant aspects in dentistry. Dent Mater. 2010;26:807-20.
https://doi.org/10.1016/j.dental.2010.04.006
PMid:20537701

 

8. Bachhav VC, Aras MA. Zirconia-based fixed partial dentures: A clinical review. Quintessence Int. 2011;42:173-82.
PMid:21359252

 

9. Stawarczyk B, Özcan M, Hallmann L, Ender A, Mehl A, Hammerlet C. The effect of zirconia sintering temperature on flexural strength, grain size, and contrast ratio. Clin Oral Invest. 2013;17:269-74.
https://doi.org/10.1007/s00784-012-0692-6
PMid:22358379

 

10. Jiang L, Liao Y, Wan Q, Li W. Effects of sintering temperature and particle size on the translucency of zirconium dioxide dental ceramic. J Mater Sci Mater Med. 2011;22:2429-35.
https://doi.org/10.1007/s10856-011-4438-9
PMid:21922331

 

11. Tholey MJ, Swain MV, Theil N. Thermal gradients and residual stresses in veneered Y-TZP frameworks. Dent Mater. 2011;27:1102-10.
https://doi.org/10.1016/j.dental.2011.08.001
PMid:21907400

 

12. Keuper M, Eder K, Berthold C, Nickel KG. Direct evidence for continuous linear kinetics in the low-temperature degradation of Y-TZP. Acta Biomater. 2013;9:4826-35.
https://doi.org/10.1016/j.actbio.2012.08.032
PMid:22925608

 

13. Coli P, Karlsson S. Precision of a CAD/CAM technique for the production of zirconium dioxide copings. Int J Prosthodont. 2004;17:577–80.
PMid:15543914

 

14. Tinschert J, Natt G, Mautsch W, Spiekermann H, Anusavice KJ. Marginal fit of alumina-and zirconia-based fixed partial dentures produced by a CAD/CAM system. Oper Dent. 2001;26:367–74.
PMid:11504436

 

15. Denry I, Kelly JR. State of the art of zirconia for dental applications. Dent Mater. 2008;24:299-307.
https://doi.org/10.1016/j.dental.2007.05.007
PMid:17659331

 

16. Reich S, Wichmann M, Nkenke E, Proeschel P. Clinical fit of all-ceramic three-unit fixed partial dentures, generated with three different CAD/CAM systems. Eur J Oral Sci. 2005;113:174–79.
https://doi.org/10.1111/j.1600-0722.2004.00197.x
PMid:15819826

 

17. Marinis A, Aquilino SA, Lund PS, Gratton DG, Stanford CM, Diaz-Arnold AM, et al. Fracture toughness of yttria-stabilized zirconia sintered inconventional and microwave ovens. J Prosthet Dent. 2013;109:165-71.
https://doi.org/10.1016/S0022-3913(13)60037-2

 

18. Miyazaki T, Nakamura T, Matsumura H, Ban S, Kobayashi T. Current status of zirconia restoration. J Prosthodont Res. 2013;5:236-61.
https://doi.org/10.1016/j.jpor.2013.09.001
PMid:24140561

 

19. Sailer I, Feher A, Filser F, Gauckler LJ, Luthy H, Hammerle CH. Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prosthodont. 2007;20:383-8.
PMid:17695869

 

20. Traini T, Sorrentino R, Gherlone E, Perfetti F, Bollero P, Zarone F. Fracture strength of zirconia and alumina ceramic crowns supported by implants. J Oral Implantol. 2015;41:352-9.
https://doi.org/10.1563/AAID-JOI-D-13-00142
PMid:24779915

 

21. Zhang Y, Lee JJ, Srikanth R, Lawn BR. Edge chipping and flexural resistance of monolithic ceramics. Dent Mater. 2013;29:1201-8.
https://doi.org/10.1016/j.dental.2013.09.004
PMid:24139756 PMCid:PMC4000448

 

22. Wang L, D'Alpino PH, Lopes LG, Pereira JC. Mechanical properties of dental restorative materials: relative contribution of laboratory tests. J Appl Oral Sci. 2003;11:162-7.
https://doi.org/10.1590/S1678-77572003000300002
PMid:21394387

 

23. Hjerppe J, Vallittu PK, Froberg K, Lassila LV. Effect of sintering time onbiaxial strength of zirconium dioxide. Dent Mater. 2009;25:166-71.
https://doi.org/10.1016/j.dental.2008.05.011
PMid:18632146

 

24. Kim MJ, Ahn JS, Kim JH, Kim HY, Kim WC. Effects of the sinteringconditions of dental zirconia ceramics on the grain size and translucency. J AdvProsthodont. 2013; 5:161-6.
https://doi.org/10.4047/jap.2013.5.2.161

 

25. Heffernan MJ, Aquilino SA, Diaz-Arnold AM, Haselton DR, Stanford CM, Vargas MA. Relative translucency of six all-ceramic systems. Part I: core materials. J Prosthet Dent. 2002;88:4-9.
https://doi.org/10.1067/mpr.2002.126794
PMid:12239472

 

26. Chen IW, Wang XH. Sintering dense nanocrystalline ceramics without final-stage grain growth. Nature. 2000;404:168-71.
https://doi.org/10.1038/35004548
PMid:10724165

 

27. Ersoy NM, Aydogdu HM, Degirmenci BU, Cokuk N, Sevimay M. The effects of sintering temperature and duration on the flexural strength and grain size of zirconia. Acta Biomater Odontol Scand. 2015;1:43-50.
https://doi.org/10.3109/23337931.2015.1068126
PMid:28642900 PMCid:PMC5433200

 

28. Matsui K, Yoshida H, Ikuhara Y. Isothermal sintering effect on phase separation and grain growth in yttria-stabilized tetragonal zirconia polycrystal. J Am Ceram Soc. 2009;92:467-75.
https://doi.org/10.1111/j.1551-2916.2008.02861.x

 

29. Lazar DR, Bottino MC, Ozcan M, Valandro LF, Amaral R, Ussui V, et al. Y-TZP ceramic processing from coprecipitated powders: a comparative study with three commercial dental ceramics. Dent Mater. 2008;24:1676-85.
https://doi.org/10.1016/j.dental.2008.04.002
PMid:18541294

 

30. Stefanic G, Grzeta B, Popovic S, Music S. In situ Phase analysis of the thermal decomposition products of zirconium salts. Croatica Chemica Acta. 1999;72:395-412.